Competition between inclusion- and microstructure-induced fatigue failure in ultraclean 100Cr6 bearing steel

Zheng Wanga, Feng Chena, Tao Shib, Qun Zhoua,c, Yuhui Chena,d, Bin Hua, Haiwen Luoa,*   

  1. aDepartment of Ferrous Metallurgy, University of Science and Technology Beijing, Beijing 100083, China;
    bBar Research Institute, Daye Special Steel Co., Ltd., Huangshi 435001, China;
    cResearch & Development Center, CITlC Pacific Special Steel Group Co., Ltd., Jiangyin 214429, China;
    dQingdao Special Steel Co., Ltd., Qingdao 266409, China
  • Received:2025-11-25 Revised:2026-02-03 Accepted:2026-02-10 Online:2026-11-16
  • Contact: *E-mail address: luohaiwen@ustb.edu.cn (H. Luo).

Abstract: The fatigue behavior of an ultraclean 100Cr6 bearing steel produced by vacuum induction melting and vacuum arc remelting was investigated to elucidate the competing roles of inclusions and microstructure. Rotating bending fatigue tests were conducted on samples subjected to conventional quenching and tempering (QT) and gradient quenching and tempering (GQT). In the QT samples, fatigue cracks initiated at both microstructural defects and inclusions, with microstructure-induced failures dominating. The ultraclean steel exhibited an unprecedented fatigue strength of 1108 MPa after QT treatment, which further increased to 1160 MPa after GQT due to grain refinement that suppressed microstructure-induced cracking. Critical crack-initiating sizes were determined as 10.5 µm for complex inclusions, 6.1 µm for TiN, and 6.8 µm for prior austenite grain in the bearing steels. Transition boundaries among these three failure mechanisms were established and, when combined with maximum crack source sizes estimated by the Statistics of Extreme Values method, successfully predicted the dominant crack initiation sources in QT, GQT, and previously reported lower-cleanliness QT-electric arc furnace bearing steels. Furthermore, a fatigue life predictive model was developed, accurately capturing the fatigue behavior of steels with varying cleanliness levels and microstructural characteristics. These findings provide new insights into optimizing ultraclean bearing steels by controlling inclusions during steelmaking and tailoring microstructures through heat treatment to further enhance fatigue performance.

Key words: Fatigue failure, Bearing steel, Inclusion, Microstructure, Competition