J. Mater. Sci. Technol. ›› 2026, Vol. 271: 31-42.DOI: 10.1016/j.jmst.2026.01.049

• Research Article • Previous Articles     Next Articles

Damage evolution and fracture mechanisms of Al-Cu-Li alloy during elevated-temperature tensile deformation via in-situ synchrotron tomography

Fuyuan Liua, Zelong Dua, Guantao Wanga, Enyu Guoa,b,*, Zongning Chena,b, Yanjin Xuc, Zhirou Zhanga, Huijun Kanga,b, Tongmin Wanga,b,*   

  1. aKey Laboratory of Solidification Control and Digital Preparation Technology (Liaoning Province), School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China;
    bNingbo Institute of Dalian University of Technology, Ningbo 315000, China;
    cAVIC Manufacturing Technology Institute, Beijing 100024, China
  • Received:2025-10-29 Revised:2026-01-05 Accepted:2026-01-05 Online:2026-02-06
  • Contact: *E-mail addresses: . eyguo@dlut.edu.cn (E. Guo), tmwang@dlut.edu.cn (T. Wang)

Abstract: Al-Cu-Li alloys are widely applied in aerospace and military owing to their high specific strength and stiffness. However, their mechanical behavior under elevated-temperature environments is degraded, with reduced strength and damage tolerance. This study investigates the microstructural evolution and damage mechanisms of Al-4.1Cu-1.3Li-0.4Mg-0.4Ag-0.5Zn-0.3Mn-0.1Zr alloy under elevated-temperature tensile loading. In-situ synchrotron tomography is performed during tensile tests at varying temperatures (100- 200 °C) to reveal the mechanical performance and damage mechanisms. As the tensile temperature in- creases, both the yield strength and ultimate tensile strength decrease from 694 to 739 MPa at 25 °C to 501 and 521 MPa at 200 °C, while elongation increases from 5.9 % to 12.0 %. The strength reduction is primarily attributed to the dissolution and coarsening of T1 precipitates, with the accelerated coarsening rate as the temperature rises. Concurrently, the geometrically necessary dislocation density decreases, and the precipitate-free zones widen, promoting strain localization and crack initiation at grain boundaries. In-situ synchrotron tomography reveals that voids predominantly nucleate near the T phase. At 100 °C, brittle fracture initiates from the T phase, followed by the nucleation of voids at these regions, which grow slowly into elliptical shapes along the loading direction. As the temperature increases to 200 °C, the interface strength between the T phase and matrix reduces, leading to debonding and a dominant void nucleation mechanism. Voids continue to grow and merge through plastic necking, ultimately re- sulting in intergranular ductile fracture.

Key words: Al-Cu-Li alloys, Fracture mechanisms, Dynamic evolution, In-situ synchrotron tomography