J. Mater. Sci. Technol. ›› 2026, Vol. 272: 227-240.DOI: 10.1016/j.jmst.2026.02.024

• Research Article • Previous Articles     Next Articles

Regulating stress-induced martensitic transformation through primary α phase to enhance work hardening in a Ti-7Mo-3Al-3Cr-3Nb alloy

Xiaoyong Zhua, Baifeng Luana,b,*, An Yana, Chenguang Baia,b, Min Zhangc, Fengwei Sund, Zhiqing Zhanga, Hongchao Koue,*   

  1. aInternational Joint Laboratory for Light Alloys (MOE), Shenyang National Laboratory for Materials Science, College of Materials Science and Engineering, Chongqing University, Chongqing 400044, China;
    bMingyue Lake Laboratory, Chongqing University, Chongqing 400044, China;
    cNew Copper-based Materials Industry Generic Technology Research Center of Anhui Province, College of Mechanical Engineering, Tongling University, Tongling 244000, China;
    dCollege of Aeronautics and Astronautics, Chongqing University, Chongqing 400044, China;
    eState Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi’an 710072, China
  • Received:2025-10-24 Revised:2026-02-19 Accepted:2026-02-19 Online:2026-11-16
  • Contact: *E-mail addresses: bfluan@cqu.edu.cn (B. Luan), hchkou@nwpu.edu.cn (H. Kou).

Abstract: Metastable β titanium alloys can achieve enhanced ductility through transformation-induced plasticity (TRIP) and/or twinning-induced plasticity (TWIP); however, their work-hardening rates are typically limited to ∼1-3 GPa, constraining further strengthening. In this study, a Ti-7Mo-3Al-3Cr-3Nb (wt.%) alloy with tailored primary α-phase fractions, achieved via a simple heat treatment in the α+β phase field, exhibits an ultrahigh work-hardening rate of up to ∼12.8 GPa. Meanwhile, the TRIP effect is preserved, resulting in a reasonable tensile elongation of ∼16 %. This mechanical response is associated with a uniform distribution of primary α phase within the β matrix, which modulates the stability of the retained β phase and governs the activation of stress-induced martensitic transformation. During deformation, the progressive activation of multiple α″ martensite variants, together with martensitic twinning, refines the retained β matrix and gives rise to a pronounced dynamic Hall-Petch effect at intermediate strains. At higher strain levels, the development of martensitic domains and additional twinning modes contributes to sustained plastic deformation and delayed strain localization. Meanwhile, the coordinated activation of 〈a〉 and 〈c+a〉 slip in the primary α phase improves deformation compatibility. These results demonstrate an effective microstructural pathway to enhance strain hardening in metastable β titanium alloys through controlled β→α″ martensitic transformation.

Key words: Metastable β titanium alloys, Work-hardening rates, Stress-induced α″ martensitic transformation, Transformation-induced plasticity