J. Mater. Sci. Technol. ›› 2026, Vol. 271: 279-286.DOI: 10.1016/j.jmst.2026.02.018

• Research Article • Previous Articles     Next Articles

Core-shell structural engineering for efficient τ f regulation in low-loss MgF2-based microwave dielectric ceramics

Jing Ye Jina,b, Mo Weia,b, Yu Hui Huangc,*, Qing Wei Zhoua,d, Kai Xin Songb,*, Bing Liua,b,e,*   

  1. aKey Laboratory of Micro-nano Sensing and IoT of Wenzhou, Wenzhou Institute of Hangzhou Dianzi University, Wenzhou 325038, China;
    bCollege of Electronic Information and Engineering, Hangzhou Dianzi University, Hangzhou 310018, China;
    cSchool of Materials Science and Engineering, Zhejiang University, Hangzhou 310058, China;
    dCollege of Materials and Environmental Engineering, Hangzhou Dianzi University, Hangzhou 310018, China;
    eZhejiang Key Laboratory of Optoelectronic Intelligent Imaging and Aerospace Sensing, Hangzhou Dianzi University, Hangzhou 310018, China
  • Received:2026-01-16 Revised:2026-02-15 Accepted:2026-02-15 Online:2026-03-05
  • Contact: *E-mail addresses:huangyuhui@zju.edu.cn (Y.H. Huang), kxsong@hdu.edu.cn (K.X. Song), liubing@hdu.edu.cn (B. Liu)

Abstract: Achieving a near-zero temperature coefficient of resonant frequency ( τ f ) while maintaining high quality factor ( Q ), typically reported as Q × f ( Qf ), in microwave dielectric ceramics is a significant challenge. In this work, a core-shell structural engineering strategy is proposed for efficient τ f regulation in MgF2 - 0.5 wt% LiF (MFL0.5) ceramics, which exhibit excellent microwave dielectric performance ( εr = 5.09, Qf = 100,733 GHz) but suffer from a large negative τ f (-67.4 ppm/ °C). Instead of dispersing temperature- compensation phases throughout the matrix, a pre-densified TiO2 ceramic with positive τ f is introduced as a compact core embedded within the MFL0.5 shell, forming an integrated core-shell architecture. Experimental results show that a near-zero τ f of -1.97 ppm/ °C can be achieved with only ∼1.27 wt% TiO2 , while retaining a high Qf value of 50,302 GHz. In contrast, conventional MFL0.5-TiO2 composite ceramics require 20 wt% TiO2 to achieve similar τ f compensation, resulting in a significant decrease in Qf to 25,933 GHz. Electric-field distribution simulations highlight the enhanced electric filling factor of the TiO2 core, which plays a key role in efficient τ f regulation. This core-shell architecture provides a highly ef- fective strategy for regulating τ f with minimal dielectric loss penalty, offering a promising pathway for the development of high-performance, low- εr microwave dielectric ceramics for advanced communica- tion systems.

Key words: Temperature coefficient of resonant frequency, Core-shell architecture, Microwave dielectric ceramics