J. Mater. Sci. Technol. ›› 2026, Vol. 271: 157-166.DOI: 10.1016/j.jmst.2026.02.008

• Research Article • Previous Articles     Next Articles

Tailoring interdiffusion and enabling self-healing for superior oxidation resistance in TiAlCrNbY coatings

Tianfang Suna,b,1, Yang Chena,c,1, Pan Yinga,1, Xin Zhongb, Yaran Niub,*, Zhixiang Qia, Xuebin Zhengb,*, Guang Chena,*   

  1. aState Key Laboratory of Light Superalloys (HAUST) / Advanced Casting Technologies, Nanjing Belight Laboratory, Nanjing University of Science and Technology, Nanjing 210094, China;
    bKey Laboratory of Inorganic Coating Materials CAS, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai 200050, China;
    cInner Mongolia North Heavy Industries Group Corporation Limited, Inner Mongolia 014000, China
  • Received:2025-07-29 Revised:2026-02-03 Accepted:2026-02-03 Online:2026-02-12
  • Contact: *E-mail addresses:yrniu@mail.sic.ac.cn (Y. Niu), xbzheng@mail.sic.ac.cn (X. Zheng), gchen@njust.edu.cn (G. Chen)
  • About author:1These authors contributed equally to this work.

Abstract: Long-term thermal stability of TiAlCr-based coatings is often compromised by interdiffusion and defect accumulation. However, strategies that simultaneously suppress interdiffusion and enable microstructural self-healing under high-temperature oxidation remain underdeveloped. Herein, we report a TiAlCrNbY coating synthesized via arc ion plating followed by controlled thermal treatment, which exhibits record-long oxidation resistance at 1000 °C for up to 300 h. Upon prolonged exposure, a dense α-Al2O3 scale formed, while internal Al2O3 precipitates emerged at microvoids, promoting defect sealing. These precipitates later dissolved and reacted with segregated Y, driven by oxygen potential gradients, forming Y3Al5O12 particles that acted as oxygen scavengers and volumetric stabilizers. Concurrently, the initial AlCr2 transformed into a stable Ti(Al, Cr)2 Laves phase, which, along with γ-TiAl, formed a dense matrix that restricted further diffusion. The interdiffusion zone showed minimal growth between 50 and 300 h (∼47-∼50 μm), indicating effective suppression of substrate-coating reactions. This self-healing behavior, together with the phase-stabilized suppression of interdiffusion, ensures long-term microstructural and chemical stability of the coating. The demonstrated synergy between oxidation-induced phase evolution and diffusion control offers a promising framework for next-generation high-temperature protective coatings.

Key words: TiAlCr-based coating, Arc ion plating, Oxidation resistance, Self-healing, Interdiffusion, Phase evolution