J. Mater. Sci. Technol. ›› 2023, Vol. 157: 174-188.DOI: 10.1016/j.jmst.2023.01.047

• Research Article • Previous Articles     Next Articles

A new strengthening mechanism driven by disruptive shear and solute segregation during warm rolling in 1.4 GPa class 12.5 wt% Al added-FeMnC ultra-lightweight steel

Chiwon Kima, Hyun-Uk Honga,*, Joonoh Moona, Bong Ho Leeb, Seong-Jun Parkc, Chang-Hoon Leec   

  1. aDepartment of Materials Convergence and System Engineering, Changwon National University 20 Changwondaehak-ro, Changwon, Gyeongnam 51140, Republic of Korea;
    bAdvanced Analysis Team, Daegu Gyeongbuk Institute of Science and Technology 333 Technojungang-daero, Daegu, 42988, Republic of Korea;
    cFerrous Alloy Department, Korea Institute of Materials Science 797 Changwondaero, Changwon, Gyeongnam 51508, Republic of Korea
  • Received:2022-08-31 Revised:2022-08-31 Accepted:2022-08-31 Published:2023-09-10 Online:2023-09-07
  • Contact: *E-mail address: huhong@changwon.ac.kr (H.-U. Hong).

Abstract: Novel strengthening of Fe‒29.1Mn‒12.5Al‒1.35C‒4.95Cr steel achieved by warm rolling was investigated. The solution-treated steel consisted of a γ-matrix containing nano-sized κ-carbide ((Fe,Mn)3AlC) and elongated prior ferrite, which was transformed into FeAl-type B2 and Fe3Al-type D03 phases. The solution-treated steel exhibited poor strain hardening owing to glide softening associated with κ-carbide shearing by dislocations. However, after warm rolling with a reduction ratio of 30% at 300 °C, the yield and tensile strengths significantly increased from 917 to 1300 MPa and 1025 to 1419 MPa, respectively. The tensile test conducted at 300 °C to simulate warm rolling exhibited serrated flows, indicating dynamic strain aging (DSA). Atom probe tomography exhibited that the C atoms in κ-carbide were swept away along the slip direction by disruptive shear during rolling at 300 °C. The swept C atoms along the slip direction interacted strongly with dislocations at 300 °C, with repeated pinning and breakaway of dislocations from the C atoms. This contributed to significant strengthening owing to the formation of a solute-rich atmosphere after warm rolling. The results of the tensile tests at 300 °C indicated that the degree of strengthening was proportional to the pre-strain level. Tensile strength of 1.4 GPa can be achieved with good ductility (17% elongation) by warm rolling. This novel warm-rolling strengthening method expedites the potential application of Fe‒29.1Mn‒12.5Al‒1.35C‒4.95Cr as a 1.4 GPa class ultra-lightweight steel.

Key words: FeMnAlC, Cr addition, κ-carbide, Dynamic strain aging, Strengthening