Effects of rejuvenation heat treatment on microstructure and creep property of a Ni-based single crystal superalloy
|
K.J. Tan, X.G. Wang, J.J. Liang, J. Meng, Y.Z. Zhou, X.F. Sun
|
|
|
Table 3 The composition of each region and precipitated phase (wt%).
|
|
Location | Ni | Co | Cr | W | Ta | Mo | Re | Al | O | Surface precipitate (H) | 21.17 | 2.53 | 20.93 | 22.09 | 19.63 | 6.12 | 1.78 | 0.05 | 5.71 | γ'-free layer (B) | 64.27 | 7.90 | 8.68 | 4.79 | 10.41 | 1.17 | 1.93 | 0.84 | — | Transition layer (D) | 68.87 | 8.92 | 8.12 | 5.64 | 2.26 | 1.77 | 2.85 | 1.59 | — | Interior (G) | 61.73 | 10.19 | 7.78 | 8.35 | 5.42 | 0.92 | 2.91 | 2.70 | — | Inside precipitate (I) | 25.52 | 2.04 | 11.01 | 25.13 | 20.16 | 7.20 | 8.91 | 0.01 | — |
|
|
|