Processing soft ferromagnetic metallic glasses: on novel cooling strategies in gas atomization, hydrogen enhancement, and consolidation
|
. |
Fig. 7.. Saturation magnetization determined from vibrating sample magnetometer measurements as a function of particle size for (a) {(Fe0.6Co0.4)0.75B0.2Si0.05}96Nb4 and (b) Fe76B10Si9P5 powders. Conventional gas atomization and novel cooling strategies were considered for this study. Measurements on melt spinning samples (MS) were also plotted for comparison (the dashed line refers to the average saturation magnetization and the upper and lower edges of the orange area defines the upper and lower standard deviation). |
![]() |