Mechanistic study of ammonium-induced corrosion of AZ31 magnesium alloy in sulfate solution
|
. |
Fig. 6.. Surface morphologies of AZ31 magnesium alloy without corrosion products after immersion in the solutions containing 0.001 M (a1)-(a3), 0.01 M (b1)-(b3), and 0.1 M (c1)-(c3) NH4+ for 6 h (a1)-(c1), 24 h (a2)-(c2), and 120 h (a3)-(c3). |
![]() |