Exceptional mechanical properties of AZ31 alloy wire by combination of cold drawing and EPT
|
|
Zhaohui Shan, Jing Bai, Jianfeng Fan, Hongfei Wu, Hua Zhang, Qiang Zhang, Yucheng Wu, Weiguo Li, Hongbiao Dong, Bingshe Xu
|
|
| |
Table 1 Electropulsing parameters of samples.
|
|
| Sample No. | Frequency, f (Hz) | Pulse width, τp(μs) | Current density, Jm (A/m2) | Duty ratio | Processing time, t (s) | | 1 | 100 | 20 | 1.88 × 1010 | 0.0020 | 180 | | 2 | 100 | 20 | 1.88 × 1010 | 0.0020 | 300 | | 3 | 100 | 20 | 1.88 × 1010 | 0.0020 | 600 | | 4 | 100 | 25 | 1.88 × 1010 | 0.0025 | 180 | | 5 | 100 | 25 | 1.88 × 1010 | 0.0025 | 300 | | 6 | 100 | 25 | 1.88 × 1010 | 0.0025 | 600 | | 7 | 100 | 30 | 1.88 × 1010 | 0.0030 | 30 | | 8 | 100 | 30 | 1.88 × 1010 | 0.0030 | 60 | | 9 | 100 | 30 | 1.88 × 1010 | 0.0030 | 180 |
|
|
|