Microstructural evolution and FCC twinning behavior during hot deformation of high temperature titanium alloy Ti65
Zhixin Zhanga,c, Jiangkun Fana,b,*(), Bin Tanga,b, Hongchao Koua,b, Jian Wangc, Xin Wangc, Shiying Wangd, Qingjiang Wange, Zhiyong Chene, Jinshan Lia,b,*()

.

Fig. 10.. IPF and the corresponding PF of Ti65 alloy deformed at 1080℃ and 0.1s-1 with different true strain: (a) (b) 0.04; (c) (d) 0.4; (e) (f) 0.7.