Microstructural evolution and FCC twinning behavior during hot deformation of high temperature titanium alloy Ti65
Zhixin Zhanga,c, Jiangkun Fana,b,*(), Bin Tanga,b, Hongchao Koua,b, Jian Wangc, Xin Wangc, Shiying Wangd, Qingjiang Wange, Zhiyong Chene, Jinshan Lia,b,*()

.

Fig. 9.. (a) Flow stress-strain curve with the corresponding microstructure of Ti65 alloy deformed at 1080 ℃ and 0.1 s-1 with different true strain: (b) 0.04; (c) 0.4; (d) 0.7.