Deformation twinning in equiaxed-grained Fe-6.5 wt.%Si alloy after rotary swaging
|
. |
Fig. 6.. Orientation maps of the specimens after SQ at 800 °C×10 min (a), after BQ at 800 °C×10 min (b), and corresponding legend (c) for maps. |
![]() |