Deformation twinning in equiaxed-grained Fe-6.5 wt.%Si alloy after rotary swaging
Chaoyu Hana, Shibo Wena, Feng Yea,*(), Wenjia Wub, Shaowei Xuea, Yongfeng Lianga, Binbin Liua, Junpin Lina

.

Fig. 2.. Fracture morphology of specimens (a) before and after heat treatments: (b) BQ at 800 °C × 5 min, (c) WQ at 800 °C × 10 min, and (d) SQ at 850 °C × 5 min.