Deformation twinning in equiaxed-grained Fe-6.5 wt.%Si alloy after rotary swaging
Chaoyu Han, Shibo Wen, Feng Ye, Wenjia Wu, Shaowei Xue, Yongfeng Liang, Binbin Liu, Junpin Lin
Table 7 Heat treatments of Φ6 mm bars.
Cooling methods Technical parameters
Brine quenching (BQ) 800 °C ×10 min 800 °C ×1 h 800 °C ×5 h 800 °C ×10 h
Furnace cooling (FC) 800 °C ×10 min 800 °C ×1 h 800 °C ×5 h 800 °C ×10 h