Numerical simulation for dendrite growth in directional solidification using LBM-CA (cellular automata) coupled method
|
|
Wonjoo Lee, Yuhyeong Jeong, Jae-Wook Lee, Howon Lee, Seong-hoon Kang, Young-Min Kim, Jonghun Yoon
|
|
| |
Table 5 Material properties of Ni-based superalloy [53,54].
|
|
| Property and symbol | Value | Units | | Density, ρ | 8.780×103 | kg m-3 | | Solute diffusivity in liquid, Dl | 3.6×10-9 | m2 s-1 | | Gibbs-Thomson coefficient, Γ | 3.65×10-7 | mK | | Partition coefficient, k0 | 0.788 | | | Liquidus slope, mL | -3.95 | K wt%-1 | | Liquidus temperature, Teq | 1672 | K | | Initial composition, C0 | 37.0 | wt% | | Anisotropy coefficient, ε | 0.02 | | | Viscosity, μ | 8.5×10-3 | kg m-1 s-1 |
|
|
|