A simultaneous improvement of both strength and ductility by Sn addition in as-extruded Mg-6Al-4Zn alloy
|
Xiao-Yuan Wang, Yu-Fei Wang, Cheng Wang, Shun Xu, Jian Rong, Zhi-Zheng Yang, Jin-Guo Wang, Hui-Yuan Wang
|
|
|
Table 4 Average Schmid factors calculated from the inverse pole figures of AZ64 and AZT643 samples at different tensile stages along ED.
|
|
| AZ64 | AZT643 | | Non-deformed | 8% deformed | Variation (%) | Non-deformed | 8% deformed | Variation (%) | Basal <a> | 0.3 | 0.312 | 4 | 0.339 | 0.236 | -30.4 | Prismatic <a> | 0.138 | 0.146 | 5.8 | 0.161 | 0.082 | -49 | Pyramidal <a> | 0.276 | 0.274 | -0.7 | 0.301 | 0.203 | -32.6 | Pyramidal <c+a> | 0.396 | 0.386 | -2.5 | 0.369 | 0.442 | 19.8 |
|
|
|