Methanogenic archaea and sulfate reducing bacteria induce severe corrosion of steel pipelines after hydrostatic testing
Enze Zhou, Jianjun Wang, Masoumeh Moradi, Huabing Li, Dake Xu, Yuntian Lou, Jinheng Luo, Lifeng Li, Yulei Wang, Zhenguo Yang, Fuhui Wang, Jessica A. Smith
Table 4 Corrosion parameters obtained from dynamic potential polarization curves of X52 steel coupons exposed to GW or LW for 14 and 30 days, respectively.
icorr (A/cm2) Ecorr (V) vs. SCE
14 days
GW 2.58 × 10-6 -0.719
LW 1.74 × 10-5 -0.738
30 days
GW 6.56 × 10-6 -0.903
LW 1.48 × 10-5 -0.848