Laser ablation and structuring of CdZnTe with femtosecond laser pulses
|
. |
Fig. 5.. Sequence of SEM images displaying the evolution of the LIPSS formed on sample surface after irradiation with (a) N = 300, (b) N = 500 and (c) N = 1000 laser pulses at E = 55 μJ. The double headed arrow in panel (a) represents the direction of laser polarization. |
![]() |