Laser ablation and structuring of CdZnTe with femtosecond laser pulses
J.J.J. Nivasa,b, E. Allahyaria,b, A. Vecchionec, Q. Haod, S. Amorusoa,b, X. Wangb,e,*()

.

Fig. 2.. (a) SEM image of the CdZnTe surface after the irradiation with N = 20 pulses with energy E = 5 μJ (Fp = 0.64 J/cm2). The red arrow represents the laser polarization direction; (b) Zoomed view of the marked region in (a), clearly showing long cracks with nanometer width formed on the surface (see also inset); (c) 2D-FFT of the crater in (a), indicating that the cracks are formed along direction at angles multiples of π/3.