Effect of warm rolling process on microstructures and tensile properties of 10¬タノMn steel
|
. |
Fig. 5.. SEM images on the microstructures after the IA for the specimens warm rolled at 250°C (a), 400°C (b), 600°C (c), 650°C (d), 700°C (e), 750°C (f) and 800°C (g) by 50% reduction in thickness, and at 600°C (h) and 650°C (i) by 63%. The 'a' and 'P' in images represent ferrite and pearlite. |
![]() |