Effect of warm rolling process on microstructures and tensile properties of 10¬タノMn steel
|
. |
Fig. 4.. EBSD band contrast images overlapped by phase distribution on the microstructures of specimens warm rolled at 250°C (a), 600°C (b) and 800°C (c) with 50% reduction in thickness; and at 600°C with 63% (d). The green in images represent austenite; the ‘a’ represents martensite. |
![]() |