Microstructural features of biomedical cobalt-chromium-molybdenum (CoCrMo) alloy from powder bed fusion to aging heat treatment
|
|
Haoqing Li, Ming Wang, Dianjun Lou, Weilong Xia, Xiaoying Fang
|
|
| |
Table 3 EDS results of different areas corresponding to Fig. 7.
|
|
| No. | Phase | Co | Cr | Mo | W | Si | | 1 | Matrix | 62.12 | 25.95 | 5.09 | 6.52 | 0.68 | | 2 | Matrix | 61.12 | 27.07 | 4.96 | 6.03 | 0.81 | | 3 | Matrix | 63.52 | 25.46 | 5.03 | 4.98 | 1.01 | | 4 | Matrix | 61.56 | 28.13 | 4.62 | 4.08 | 1.61 | | 5 | Microsegregation zone | 57.97 | 24.02 | 5.87 | 11.07 | 1.07 | | 6 | Microsegregation zone | 57.20 | 25.65 | 5.55 | 10.98 | 0.62 | | 7 | Microsegregation zone | 56.40 | 24.82 | 5.65 | 12.23 | 0.90 | | 8 | Microsegregation zone | 59.13 | 24.01 | 6.21 | 9.90 | 0.75 | | 9 | Laves | 42.50 | 18.01 | 10.13 | 22.92 | 6.44 | | 10 | Sigma | 42.60 | 34.98 | 14.12 | 7.32 | 0.98 |
|
|
|