Microstructural features of biomedical cobalt-chromium-molybdenum (CoCrMo) alloy from powder bed fusion to aging heat treatment
Haoqing Li, Ming Wang, Dianjun Lou, Weilong Xia, Xiaoying Fang
Table 2
SLM setup and process parameters.
Layer power
Spot size
Scan speed
Layer thickness
Preheating
Scan spacing
195 W
100 μm
1200 mm/s
20 μm
80 °C
90 μm