Enhanced Strength and Ductility Due to Microstructure Refinement and Texture Weakening of the GW102K Alloy by Cyclic Extrusion Compression |
Lin Jinbao,Wang Xinyi,Ren Weijie,Yang Xuexia,Wang Qudong |
Fig. 7. Effect of CEC deformation temperature and pass number on the tensile properties of GW102K alloy: (a) ultimate tensile strength; (b) yield strength; (c) elongation-to-fracture. |
![]() |