Hydrogen-induced Modification in the Deformation and Fracture of a Precipitation-hardened Fe-Ni Based Austenitic Alloy
Mingjiu Zhao
1,
*
, Zifeng Guo
2
, Shenghu Chen
1
, Hao Liang
3
, Lijian Rong
1,
**
Fig. 3 TEM micrographs of dislocation morphology near the fracture: a without hydrogen, b with hydrogen.