Microstructure and Strength of Al2O3/Al2O3 Joints Bonded with ZnO-Al2O3-B2O3-SiO2 Glass-Ceramic
Weiwei Zhu, Jichun Chen, Chuanyong Hao, Jinsong Zhang*
Fig. 2. XRD patterns of the glass treated at different temperature: a 780 #cod#x000b0;C; b 920 #cod#x000b0;C; c 1120 #cod#x000b0;C.