Plastic Flow of a Cu50Zr45Ti5 Bulk Metallic Glass Composite
Wang G.1,*, Pauly S.2, Gorantla S.2, Mattern N.2, Eckert J.2,3
Fig. 4. TEM images of three fractured samples: a high-resolution image of the fractured CZT I sample, b dark field image and the according SAED pattern of the fractured CZT I sample, c high-resolution image of the fractured CZT II sample, d dark field image and the SAED pattern of the fractured CZT II sample, e high-resolution image of CZT III after fracture, f dark field image and the SAED pattern of the fractured CZT III specimen.