Microstructural Evolution and Mechanical Behaviour of Metastable Cu–Zr–Co Alloys
Pauly S.1,*, Kosiba K.1, Gargarella P.1, Escher B.1, Song K.K.1, Wang G.2, Kühn U.1, Eckert J.1,3
Fig. 1. XRD patterns of a the ingots of i Cu 40 Zr 37.5 Co 22.5 , ii Cu 42.5 Zr 45 Co 12.5 and iii Cu 49 Zr 49 Co 2 . b XRD patterns of the rods with a diameter of 2 mm of i Cu 40 Zr 37.5 Co 22.5 , ii Cu 42.5 Zr 45 Co 12.5 and iii Cu 49 Zr 49 Co 2 . Please note that the strongest reflection of i and ii in a and b at around 2 θ = 17.8° has been cut off.