Corrosion Behavior of X52 Anti-H
2
S Pipeline Steel Exposed to High H
2
S Concentration Solutions at 90 °C
Liu Meng, Wang Jianqiu
*
, Ke Wei, Han En-Hou
Fig. 2. XRD patterns for the corrosion products formed after different immersion time at 90 °C, in 1.61 MPa H 2 S solution.