Crystallization of Al-based Amorphous Alloys in Good Conductivity Solution
Yonggang Wang
1
, Yan Liu
1
, Yingjie Li
1
, Bang An
1
, Guanghui Cao
2
, Shifeng Jin
3
, Yimin Sun
1
, Weimin Wang
1
Fig. 6 XRD patterns of the immersed Al94-xNixGd6 x = 6 and 10 sample with: a Rc = 29.3 ms, b 25.6 ms.