Crystallization of Al-based Amorphous Alloys in Good Conductivity Solution
Yonggang Wang1, Yan Liu1, Yingjie Li1, Bang An1, Guanghui Cao2, Shifeng Jin3, Yimin Sun1, Weimin Wang1
Fig. 4 SEM micrographs of free surfaces of the Al94-xNixGd6 x = 6 and 10 glassy ribbons by electrochemical corrosion in 7 wt% HNO3 methanol solution: a Rc = 29.3 ms and x = 6; b Rc = 29.3 ms and x = 10; c Rc = 25.6 ms and x = 6; d Rc = 25.6 ms and x = 10. The film matrix is labeled as F and the particles are labeled as P for the EDS region.