Oxidation Behaviors of C-ZrB2-SiC Composite at 2100 °C in Air and O2
Zhongwei Zhang1,2, Cewen Nan1, Jingjun Xu3, Zenghua Gao3, Meishuan Li3, Junshan Wang2
Fig. 6. Illustration of the oxidation progress of G a and GZS b at 2100 #cod#x000b0;C, showing the inward diffusion of oxygen and the outward diffusion of CO during oxidation.