Oxidation Behaviors of C-ZrB2-SiC Composite at 2100 °C in Air and O2
Zhongwei Zhang1,2, Cewen Nan1, Jingjun Xu3, Zenghua Gao3, Meishuan Li3, Junshan Wang2
Fig. 5. Cross section morphologies of the oxide scales formed on GZS after oxidation at 2100 #cod#x000b0;C for 540 s: a in 1 #cod#x000D7; 105 Pa air, b in 0.2 #cod#x000D7; 105 Pa O2.