Oxidation Behaviors of C-ZrB2-SiC Composite at 2100 °C in Air and O2 |
Fig. 4. a and b surface morphologies of the oxide scale formed on GZS after oxidation at 2100 #cod#x000b0;C for 540 s in 1 #cod#x000D7; 105 Pa air, c EDS result obtained at the yellow cross in b. |
![]() |