Characteristics of Twin Lamellar Structure in Magnesium Alloy during Room Temperature Dynamic Plastic Deformation |
Fig. 4. Misorientation angle distributions of AZ31 samples with different strains: a ε = 2.1%, b ε = 4.3%, c ε = 6.5%, d ε = 8.3%. The rotation axis distributions in the crystal coordinate system indicate the different misorientation relationships. |
![]() |