Fluoride Conversion Coating on Biodegradable AZ31B Magnesium Alloy
Yan Tingting1,*, Tan Lili2, Zhang Bingchun2, Yang Ke2
Fig. 11. XRD patterns on surface of the fluoride coated AZ31B after immersion in the simulated blood plasma for 90 days: a fluoride coated AZ31B, b Mg JCPDS89-5003, c HA JCPDS09-0432, d MgF2 JCPDS 38-0882, e MgO JCPDS87-0652.