Quick-homogeneous Corrosion of Ti-2A1-2.5Zr Alloy in High-temperature and High-pressure Water Steam

Lin YANG, Zhentao YU, Ju DENG   

  1. Northwest institute for Nonferrous Metal Research, Xi'an 710016, China
  • Received:2000-04-05 Revised:1900-01-01 Online:2001-01-28 Published:2009-10-10
  • Contact: Lin YANG

Abstract: The corrosion behavior of Ti-2A1-2.5Zr alloy with 5 alloy contents and 5 surface states were studied in water steam at 400℃, 10.3 MPa for 72 h. The weight-increments of all samples are under 4 mg/dm2, better than Zr and Zr-alloy. α-Ti is oxidized into anatase-type TiO2 preferentially. The corrosion resistance is improved by adding Al element or pre-oxidizing treatment, the latter is more effective relatively.

Key words: