J Mater Sci Technol ›› 2000, Vol. 16 ›› Issue (01): 59-62.

• Research Articles • Previous Articles     Next Articles

Microstructural features of friction-welded Ti-6Al-4V joint

Daqian SUN, Zhenan REN, Zhenfeng ZHOU, T.North, Yang ZHAI, S.Sathian   

  1. Jinn University of Technology, Changchun 130025, China...
  • Received:1999-04-12 Revised:1999-05-08 Online:2000-01-28 Published:2009-10-10
  • Contact: Zhenfeng ZHOU

Abstract: Microstructural features of friction-welded Ti-6Al-4V joint have been investigated by both optical microscope and transmission electron microscope (TEM). The microstructure of the welded joint is not uniform. It can be classified into the phase transformed region(P), the deformed region(D) and the region of unchanged base metal(B). In the phase transformed region, the microstructure consists of platelike, acicular and equiaxed alpha phase plus beta phase between them and the dislocations can be observed in some or phase particles. The equiaxed alpha phase mainly distributes in the near center of rod specimen. The quantity of platelike and acicular alpha phase and the size of the grains increase progressively along the radial direction of the rod type welded joint. In the deformed region, the grains are reoriented and the microstructure consists of the elongated alpha phase containing a lot of dislocations and intergranular beta phase.

Key words: