J. Mater. Sci. Technol. ›› 2006, Vol. 22 ›› Issue (02): 190-194.

• 论文 • 上一篇    下一篇

Microstructure Evolution and Tensile Properties of Pure Ti Subjected to Rapidly Heating and Quenching

赵伟松;张伟;郭金羽;王宝全;郭敬东;卢柯   

  1. 中科院金属所
  • 收稿日期:2004-12-29 修回日期:2005-05-11 出版日期:2006-03-28 发布日期:2009-10-10
  • 通讯作者: 赵伟松

Microstructure Evolution and Tensile Properties of Pure Ti Subjected to Rapidly Heating and Quenching

Weisong ZHAO, Wei ZHANG, Jinyu GUO, Boquan WANG, Jingdong GUO, Ke LU   

  1. Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
  • Received:2004-12-29 Revised:2005-05-11 Online:2006-03-28 Published:2009-10-10
  • Contact: Weisong ZHAO

摘要: 纯钛样品被以10e6 K/s的速度加热到beta相区,随后快速冷却.处理后,原来的等轴晶中产生了微米宽的板条亚结构.相临板条的取向差为几度.这种细板条亚结构是由于在快速加热和冷却的过程中非平衡的alpha-beta-alpha 相变而产生的.拉伸强度增加了100 MPa, 塑性保持不变.强度的提高可解释为高密度亚结构对位错运动的阻碍.

关键词: 金属, 微结构

Abstract: The pure α-Ti samples were heated at an extremely high rate (~106 K/s) to the temperature of β phase zone followed by a rapidly quenching in an electro-pulsing treatment. After the treatment, micrometer-thick lamellar substructures were generated within the original equiaxed α-Ti coarse grains. Misorientations across adjacent lamellae are of a few degrees. The ultrafine lamellar substructures originated from a non-equilibrium α-β-α' phase transformation during rapidly heating-quenching process with a short exposure time at high temperatures. Tensile strength was increased by about 100 MPa due to the formation of the ultrafine lamellar substructure while the same tensile plasticity (elongation-to-failure) was maintained relative to the original sample. The strengthening effect could be attributed to the effective blockage of dislocation motions by a high density of sub-boundaries.

Key words: Pure Ti, Microstructure, Properties, Rapidly heating