CORROSION BEHAVIOR OF EPOXY-POLYAMIDE COATED CARBON STEEL IN THE WASTE PERCOLATE
ZHOU Debi1;CUI Lili1;LI Lin1;QU Junlin2;HU Jianwen1;LAI Yuan1
1.Institute of Chemistry and Chemical Engineering; Central South University; Changsha 410083
2.Narada Licom Power Tech. Co.; Ltd.; Shanghai 201206
Download:  PDF(4745KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The corrosion behaviors of epoxy-polyamide coated carbon steel in the mixed solution of NaCl-(NH4)2SO4-NH4Cl and in the waste percolate were investigated using polarization curve and electrochemical impedance spectroscopy (EIS) methods. The corrosion potential of the sample ranged from -0.47 V to -0.61 V in the mixed solution and from -0.60 V to -0.68 V in the waste percolate. The waste percolate showed a stronger corrosiveness than that of the mixed solution. The coating of the epoxy-polyamide exhibited a good stability and corrosion resistance in the above corrosive environment.

Key words:  waste percolate      epoxy-polyamide      corrosion      EIS      equivalent circuit     
Received:  24 April 2007     
ZTFLH: 

TG178

 
Corresponding Authors:  ZHOU Debi     E-mail:  zhoudb@mail.csu.edu.cn

Cite this article: 

. CORROSION BEHAVIOR OF EPOXY-POLYAMIDE COATED CARBON STEEL IN THE WASTE PERCOLATE. J Chin Soc Corr Pro, 2009, 29(1): 50-54.

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2009/V29/I1/50

[1] Zhang C B. Impedance models of epoxy coated LY12 aluminum alloys in NaCl solution[J]. J. Geol. Hazards Environ.Preserv.,1999,10(Supp1.):68-87
(张澄博.垃圾卫生填埋结构对地质环境效应的控制研究[J].地质灾害与环境保护,1999,10(增刊):68-87)
[2] Chen Q,Su C Y,Li Y. Study on corrosion of environment sanitary facilities[J]. Environ. Sanit. Eng.,2002,4(1):39-42
(陈全,苏春玉,李杨. 环卫设施腐蚀问题的研究[J]. 环境卫生工程,2002,4(1):39-420)
[3] Huo W Z,Dong X Q. Anti-corrosion solutions for largegarbage carrying vehicles[J]. Munic.Adm.Technol.,2002,4(4):16-17
(霍维周,董雪青. 大型垃圾转运车箱腐蚀与防护研究[J]. 城市管理与科技,2002,4(4):16-17)
[4] Jing X L,Wang Y Y,Qiang J F. Anti-corrosive property of emeraldine base form of polyaniline[J]. J.Chin. Soc. Corros. Prot.,2004,24(5):301-305
(井新利,王杨勇,强军锋.本征态聚苯胺的防腐性能[J].中国腐蚀与防护学报,2004,24(5):301-305)
[5] Shao Y W,Yan C W,Du Y L,et al. The effect of titanate coupling agent on the dispersion of the nano-Ti power in  the expoxy resin[J]. J. Chin. Soc. Corros. Prot.,2005, 25(4):232-236
(邵亚薇,严川伟,杜元龙等.钛酸酯偶联剂对纳米Ti粉在 环氧树脂中分散性的影响[J]. 中国腐蚀与防护学报,2005, 25(4):232-236)
[6] Shao Y W,Li Y,Wang F H,et al. Molecular design and synergistic effect of morpholinium type volatile corrosion inhibitor[J]. J. Chin. Soc.Corros. Prot.,2006,26(2): 115-120
(邵亚薇,李瑛,王福会等. Ti纳米粒子对环氧涂层防护性能的影响[J]. 中国腐蚀与防护学报,2006,26(2):115-120)
[7] He J,Yan R,Ma S N. Study on corrosion behaviors of epoxy coatings/substrate immersed in 3.5% NaCl solution by electrochemical methods[J]. Chin. Surf. Eng.,2006, 19(2):47-50
(何杰,阎瑞,马世宁.电化学方法研究环氧涂层/基体在3.5% NaCl溶液中的腐蚀行为[J]. 中国表面工程,2006,19(2): 47-50)
[8] Liu L W,Hu Q,Guo F. Study on destroy process of 1Cr18Ni9Ti stainless steel surface passive film by hydrogen sulfide[J]. J. Chin. Soc. Corros. Prot.,2002,22(1):22-26
(刘烈炜,胡倩,郭风. 硫化氢对不锈钢表面钝化膜破坏的研究[J].中国腐蚀与防护学报,2002,22(1):22-26)
[9] Guo H,He X Y,Dong J,et al. Electrochemical study on the corrosion behavior of A3 steel in acid solutions with SO$_{_{2}}$[J]. J. Xihua Teachers College (Nat. Sci.),2004,25 (2):176-179
(郭红,何晓英,董军等. A3钢在含SO$_{2}$酸性溶液中腐蚀行为的电化学研究[J]. 西华师范大学学报(自然科学版),2004,25 (2):176-179)
[10] Loveday D,Peterson P,Rodgers B. Evaluation of organic coatings with electrochemical impedance spectroscopy part 2:Application of EIS to coatings[J]. J. Coat. Technol.,2004,1(10):88-93
[11] Zhou D B,Liu D P,Mo C Q,et al. Corrosion behavior of 304 stainless steel in NaCl-(NH4)2SO4- NH4Cl solution[J]. J. Chin. Soc. Corros.Prot.,2007,27(2):84-92
(周德璧,刘丹平,莫成千等. 304不锈钢在NaCl-(NH4)2- SO4-NH4Cl溶液中的腐蚀行为[J]. 中国腐蚀与防护学报, 2007,27(2):84-92)

[1] HUANG Peng, GAO Rongjie, LIU Wenbin, YIN Xubao. Fabrication of Superamphiphobic Surface for Nickel-plate on Pipeline Steel by Salt Solution Etching and Its Anti-corrosion Properties[J]. 中国腐蚀与防护学报, 2021, 41(1): 96-100.
[2] DONG Xucheng, GUAN Fang, XU Liting, DUAN Jizhou, HOU Baorong. Progress on the Corrosion Mechanism of Sulfate-reducing Bacteria in Marine Environment on Metal Materials[J]. 中国腐蚀与防护学报, 2021, 41(1): 1-12.
[3] TANG Rongmao, ZHU Yichen, LIU Guangming, LIU Yongqiang, LIU Xin, PEI Feng. Gray Correlative Degree Analysis of Q235 Steel/conductive Concrete Corrosion in Three Typical Soil Environments[J]. 中国腐蚀与防护学报, 2021, 41(1): 110-116.
[4] HAN Yuetong, ZHANG Pengchao, SHI Jiefu, LI Ting, SUN Juncai. Surface Modification of TA1 Bipolar Plate for Proton Exchange Membrane Fuel Cell[J]. 中国腐蚀与防护学报, 2021, 41(1): 125-130.
[5] ZHANG Yuxuan, CHEN Cuiying, LIU Hongwei, LI Weihua. Research Progress on Mildew Induced Corrosion of Al-alloy[J]. 中国腐蚀与防护学报, 2021, 41(1): 13-21.
[6] RAN Dou, MENG Huimin, LIU Xing, LI Quande, GONG Xiufang, NI Rong, JIANG Ying, GONG Xianlong, DAI Jun, LONG Bin. Effect of pH on Corrosion Behavior of 14Cr12Ni3WMoV Stainless Steel in Chlorine-containing Solutions[J]. 中国腐蚀与防护学报, 2021, 41(1): 51-59.
[7] BAI Yunlong, SHEN Guoliang, QIN Qingyu, WEI Boxin, YU Changkun, XU Jin, SUN Cheng. Effect of Thiourea Imidazoline Quaternary Ammonium Salt Corrosion Inhibitor on Corrosion of X80 Pipeline Steel[J]. 中国腐蚀与防护学报, 2021, 41(1): 60-70.
[8] ZUO Yong, CAO Mingpeng, SHEN Miao, YANG Xinmei. Effect of Mg on Corrosion of 316H Stainless Steel in Molten Salts MgCl2-NaCl-KCl[J]. 中国腐蚀与防护学报, 2021, 41(1): 80-86.
[9] WANG Yating, WANG Kexu, GAO Pengxiang, LIU Ran, ZHAO Dishun, ZHAI Jianhua, QU Guanwei. Inhibition for Zn Corrosion by Starch Grafted Copolymer[J]. 中国腐蚀与防护学报, 2021, 41(1): 131-138.
[10] WANG Xintong, CHEN Xu, HAN Zhenze, LI Chengyuan, WANG Qishan. Stress Corrosion Cracking Behavior of 2205 Duplex Stainless Steel in 3.5%NaCl Solution with Sulfate Reducing Bacteria[J]. 中国腐蚀与防护学报, 2021, 41(1): 43-50.
[11] SHI Kunyu, WU Weijin, ZHANG Yi, WAN Yi, YU Chuanhao. Electrochemical Properties of Nb Coating on TC4 Substrate in Simulated Body Solution[J]. 中国腐蚀与防护学报, 2021, 41(1): 71-79.
[12] ZHENG Li, WANG Meiting, YU Baoyi. Research Progress of Cold Spraying Coating Technology for Mg-alloy[J]. 中国腐蚀与防护学报, 2021, 41(1): 22-28.
[13] WEI Zheng, MA Baoji, LI Long, LIU Xiaofeng, LI Hui. Effect of Ultrasonic Rolling Pretreatment on Corrosion Resistance of Micro-arc Oxidation Coating of Mg-alloy[J]. 中国腐蚀与防护学报, 2021, 41(1): 117-124.
[14] YU Hongfei, SHAO Bo, ZHANG Yue, YANG Yange. Preparation and Properties of Zr-based Conversion Coating on 2A12 Al-alloy[J]. 中国腐蚀与防护学报, 2021, 41(1): 101-109.
[15] ZHANG Hao, DU Nan, ZHOU Wenjie, WANG Shuaixing, ZHAO Qing. Effect of Fe3+ on Pitting Corrosion of Stainless Steel in Simulated Seawater[J]. 中国腐蚀与防护学报, 2020, 40(6): 517-522.
No Suggested Reading articles found!